Electrophoretic coating for domestic microwave oven
Product Introduction :
HS-6060ALB/HS-6600 White Cationic Epoxy Electrocoat for auto is a new generation electrophoretic coating researched and developed by HLS Paint (Shanghai) Co., Ltd.
It represents modern technology of cathodic electrophoretic coating that is environment-friendly with high property and low cost. Such coating does not contain heavy metal like lead, tin, cadmium and mercury etc. It is a two-component, water-dispersed resin,meanwhile, it took in features of previous products, and can adapt galvanized steel sheet perfectly, almost can be applied to foundation coating of all metal, such as: cold and hot rolled steel sheet, galvanized steel sheet, aluminum products, zinc-aluminum alloy sheet and stainless steel sheet etc.
This product features shown below:
Excellent leveling coating,good bonding force and compatibility with plastic powder.
Strong anti-corrosion properties, good salt spray resistance workpiece edge.
Good stability of bath can adaptable for a longer updating cycl
Main ingredients:
Pigment: titanium dioxide, kaolin,antirust pigment | Neutralizing agent: organic acid |
Additives: surface active agent, prevent shrinkage cavity agent,resistance to yellowing agent |
Product quality data
Project | Technical data | Test standard | ||
Resin (HS-6060ALB) | White Paste (HS-6600) | |||
pH | 25℃ | 6.0±1.0 | —— | GB/T 9724 |
Conductivity | 25℃, μs/cm | 1400±400 | —— | HG/T 3334 |
Appearance | —— | Milky white liquid | White viscous liquid,no agglomeration | Visual |
Storage stability | No stratified state, and there were no obvious difference compared to before storage | In 5-35 ℃ temperature 1 year |
Note: pH, conductivity measurement in the resin/pure water = 1:1 dilution
Filling tank proportion and method
⑴ Bath preparation
Ratio:
Resin 750.00-1000.00
Paste 250.00
DI water 1900.00-2200.00
Total 3 3025.00-3575.00
⑵ Ripening conditions
Sample quantity: 3000-4000g
Container: 5L (Diameter 16cm)
Tank temperature:28-30 ℃
Time: 24~48Hr
Mixed conditions: impeller diameter 8cm (speed 200rpm)
(3) Coating conditions
Experimental panel: phosphated cold-rolled steel plate
Tank temperature: 28-34 ℃
Pole ratio: A/C = 1/2 ~ 1/4
Distance of electrodes: 15cm
ED time: For full immersing 1-3 minutes ( 20 seconds soft start)
Baking conditions:(165-175)℃×(20-30)min (Keeping temperature of parts coated)
Customers in the microwave oven industry:
HLS Coatings (Shanghai)Co.Ltd
Since its foundation in November 2003, HAOLISEN has been adhering
to the vision of “Advocator and Innovator of Waterborne Coating
Solutions” and committed to the development and production of
industrial electrophoretic coatings by investing lots of human,
material, energy and financial resources over more than a decade.
CORPORATE CULTURE
Corporate mission: Technological innovation, customer satisfaction, and serving the country through industry.
| ![]() |